WOCO identifies this item as YQ17 thermal spray powder, model / grade YQ17. The source size is 15–45 µm. Some source size units are inconsistent with the powder designation. Confirm the required particle size and product form against the original record.

Specifications & website prices

SpecificationOriginal website priceMOQ
15–45 µm$48.00 /KgOriginal page #legacy-1104 ↗200 Kg
15–45 µm$48.00 /KgOriginal page #legacy-1138 ↗200 Kg

Each price retains the specification, currency and unit of its source listing. Confirm current availability and delivery with WOCO.

Product overview ↓
YQ17 thermal spray powder
Product reference image

Product overview

WC-17Co · Product description & applications

Model-level information transcribed from the WOCO product overview. Listed applications are examples; suitability and coating qualification depend on your process. Reference grades are separate from the priced specifications above.

  • Agglomerated & sintered or sintered & crushed gray/black spherical or near-spherical particles, with good fluidity;
  • Maximum operating temperature 500℃;
  • High hardness, dense coating, wear-resistant particle wear, fretting wear, adhesive wear, erosion wear
  • Higher fracture toughness than WC12Co
  • Mainly used in aircraft landing gear, extrusion die, wire drawing equipment, paper roll, glass industry, crushing roll, pump sealing parts etc.

Grade specifications from the product overview

GradeParticle sizeT.C %Co %Fe %O %ProcessApparent density (g/cm³)Hall flowability (s/50g)
FB106-220–53 µm4.7-5.216.5-17.5≤0.5≤0.5Sintered & Crushed≥4 g/cm³≤25 s/50g
FB107-520–45 µm4.7-5.216.5-17.5≤0.5≤0.5Sintered & Crushed≥4 g/cm³≤25 s/50g
FB108-315–45 µm4.7-5.216.5-17.5≤0.5≤0.5Sintered & Crushed≥4 g/cm³≤25 s/50g
FA107-220–53 µm4.7-5.216.5-17.5≤0.15≤0.5Agglomerated & Sintered≥4 g/cm³≤25 s/50g
FA108-520–45 µm4.7-5.216.5-17.5≤0.15≤0.5Agglomerated & Sintered≥4 g/cm³≤25 s/50g
FA109-315–45 µm4.7-5.216.5-17.5≤0.15≤0.5Agglomerated & Sintered≥4 g/cm³≤25 s/50g
FA110-611–45 µm4.7-5.216.5-17.5≤0.15≤0.5Agglomerated & Sintered≥4 g/cm³≤25 s/50g
FA111-710–38 µm4.7-5.216.5-17.5≤0.15≤0.5Agglomerated & Sintered≥4 g/cm³≤25 s/50g
FA112-810–30 µm4.7-5.216.5-17.5≤0.15≤0.5Agglomerated & Sintered≥4 g/cm³≤25 s/50g

HVOF process reference & reported coating results

The following values belong to the stated process setup in the product overview. They are starting references, not a guarantee for other equipment, substrates, grades or production runs.

Reference process conditions

PowderWC-17Co
Process typeAgglomerated & Sintered
Particle size45-15 µm
Spraying gunJP5000
Gun barrel6 inch
Kerosene22.7 L/h
Oxygen944 L/min
Carrier gas7.5 L/min
Powder feed rate70-100 g/min
Spraying distance340-380 mm

Coating results in the overview

Hardness950-1200 HV0.3
Bonding strength>70 MPa
Deposition efficiency45-55 %
Porosity<1 %

View the original product overview ↗

Technical documents

Batch reports apply to the identified batch. Ask WOCO for documents relating to your order.

Product images & original specifications

Product Name
WC17CoWC-17Co
Category
Thermal spraying
Product Size
15–45 µm
Grade
YQ17
MOQ
200Kg
YQ17 — Product Image
Product Image
YQ17 — Product Image
Product Image

Available specifications & supply reference

Original listing information is preserved below. Stock, delivery and freight are subject to current confirmation.

These are dated supplier listings. Their original prices and validity periods are shown for reference; ask WOCO for a current quotation.

SpecificationPackagingListing date / validity
15–45 µmOn request2017-10-19 · 20days
15–45 µmOn request2017-11-03 · 20days

Original supply details

Origin
CHENGDU
Validity
20days
Area
CHENGDU
Post date
2017-10-192017-11-03

Material selection guides

All technical guides ↗

Technical support

Discuss your application, material and specification with WOCO.