Start with the wear mechanism
A shaft, valve or hydraulic component may experience abrasion, erosion or corrosion-related wear. The coating material must be considered together with the substrate, component geometry and service environment. WOCO product overviews identify tungsten-carbide composite powders for a range of surface-protection applications.
Connect powder specifications with the process
Compare the documented composition, manufacturing route, morphology and particle-size range. Agglomerated-and-sintered powders and sintered-and-crushed powders are distinct products; identical nominal chemistry does not make every powder interchangeable. Confirm the appropriate feedstock with your HVOF or plasma-spray equipment requirements.
What to share with WOCO
- Component, substrate and the observed wear problem.
- Spray process, equipment and required particle-size range.
- Required quantity, destination and applicable documentation.
Use the product pages below to inspect specifications and available documents. Historical COA samples describe the stated batch; request the documentation applicable to your order from our team.
Explore material options
WC10Co4Cr
WC10Co4Cr tungsten carbide composite powder
- Material
- WC,Co,Cr,
- Process
- Sintered & crushed
- Sizes
- 20–53 µm
WC12Co
WC12Co tungsten carbide composite powder
- Process
- Agglomerated & sintered
- Sizes
- 15–45 µm
Al2O3-13TiO2
Al2O3–13TiO2 ceramic powder
- Material
- Metco 6221
- Sizes
- 15–45 µm / 11–53 µm / 15–53 µm