Tungsten-based powders

WC-12Ni

WC-12Ni

WOCO identifies this item as WC-12Ni, model / grade WC-12Ni. The source size is Particle size pending technical verification.

Specifications & website prices

SpecificationOriginal website priceMOQ
Particle size pending technical verification$45.00 /KgOriginal page #legacy-902 ↗300 Kg

Each price retains the specification, currency and unit of its source listing. Confirm current availability and delivery with WOCO.

Conflicting particle-size information is withheld pending technical verification.

Product overview ↓
WC-12Ni
Product reference image

Product overview

WC-12Ni · Product description & applications

Model-level information transcribed from the WOCO product overview. Listed applications are examples; suitability and coating qualification depend on your process. Reference grades are separate from the priced specifications above.

  • Agglomerated & sintered gray/black spherical or near-spherical particles, with good flowability.
  • The maximum operating temperature is 500℃.
  • Hard and dense coating, wear-resistant particle wear, fretting wear, adhesive wear, corrosion wear, erosion wear;
  • Non-magnetic material
  • Ni has higher corrosion resistance than Co, and is suitable for (moisture) wet corrosion environment;
  • Mainly used in oilfield equipment, petrochemical industry, ball valve (oxidation environment), plate valve, offshore equipment and parts etc.

Grade specifications from the product overview

GradeParticle sizeT.C %Ni %Fe %O %ProcessApparent density (g/cm³)Hall flowability (s/50g)
FA125-220–53 µm5.2-6.011.5-12.5≤0.5≤0.5Agglomerated & Sintered≥3.5 g/cm³≤18 s/50g
FA126-520–45 µm5.2-6.011.5-12.5≤0.5≤0.5Agglomerated & Sintered≥3.5 g/cm³≤18 s/50g
FA127-315–45 µm5.2-6.011.5-12.5≤0.5≤0.5Agglomerated & Sintered≥3.5 g/cm³≤18 s/50g
FA128-611–45 µm5.2-6.011.5-12.5≤0.5≤0.5Agglomerated & Sintered≥3.5 g/cm³≤18 s/50g
FA129-710–38 µm5.2-6.011.5-12.5≤0.5≤0.5Agglomerated & Sintered≥3.5 g/cm³≤18 s/50g
FA130-810–30 µm5.2-6.011.5-12.5≤0.5≤0.5Agglomerated & Sintered≥3.5 g/cm³≤18 s/50g

HVOF process reference & reported coating results

The following values belong to the stated process setup in the product overview. They are starting references, not a guarantee for other equipment, substrates, grades or production runs.

Reference process conditions

PowderWC-12Ni
Process typeAgglomerated & Sintered
Particle size45-15 µm
Spraying gunJP5000
Gun barrel4 inch
Kerosene24 L/h
Oxygen900 L/min
Carrier gas8.5 L/min
Powder feed rate70-100 g/min
Spraying distance340-380 mm

Coating results in the overview

Hardness1000-1200 HV0.3
Bonding strength>70 MPa
Deposition efficiency40-50 %
Porosity<1 %

View the original product overview ↗

Technical documents

Batch reports apply to the identified batch. Ask WOCO for documents relating to your order.

Product images & original specifications

Product Name
WC-12Ni
Category
Thermal spraying
Product Size
Particle size pending technical verification
MOQ
300Kg
WC-12Ni — Product Image
Product Image

Available specifications & supply reference

Original listing information is preserved below. Stock, delivery and freight are subject to current confirmation.

These are dated supplier listings. Their original prices and validity periods are shown for reference; ask WOCO for a current quotation.

SpecificationPackagingListing date / validity
Particle size pending technical verificationOn request2017-08-10 · 180days

Original supply details

Origin
China
Validity
180days
Area
China
Post date
2017-08-10

Material selection guides

All technical guides ↗

Technical support

Discuss your application, material and specification with WOCO.